Re: [MW:20844] PWHT for Heat exchanger

Dear Rajesh,
Please consider slow heating / cooling cycles.
 
With Best Regards,
Shashank C Vagal
On Monday, 19 May 2014 4:15 AM, Rajesh <mrinmeghnsk@gmail.com> wrote:


Dear All,

We are constructing an heat exchanger which has fixed tubesheet welded to shell.

Shell Material SA 516 Gr 70
Tube Material - Cu Ni 90:10
Tubesheet - SA 266 claded with CU Ni 90:10

Customer is demanding PWHT for complete heat exchanger due to process. But we have fear for failure of tube bundle after PWHT due to differential thermal expansion.

Please comment if CODE has any reference to this?

Rajesh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...