Saturday, May 31, 2014

[MW:20939] RE: 20937] Cathodic protection

The simple answer is that it is ineffective but what are you talking about, something offshore, a pipeline onshore or some other installation.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]
Sent: 30 May 2014 15:44
To: materials welding
Subject: [MW:20937] Cathodic protection

 

Dear Expert what is effect of rain on cathodic protection 

 

Regards,

Engr.Asif Shahzad
+966591268872/+923007389793

B.E Chemical Engineering
API 510
CSWIP 3.1
BGAS LEVEL II
Lead Auditor QMS(9001-2008)
NEBOSH IGC
OSHA

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...