Dear Nishant
Hydrotest pressure is code specific. As per IBR and ASME B31.1, it is 1.5 times the design pressure, howver as per ASME B31.3., it is MINIMUM 1.5 times the design pressure and a provision of temperature correction factor has to be multiplied when hydrotesting High pressure piping

Regards
Arunabh 
Engineers India Limited

On Saturday, April 27, 2013 4:32:02 PM UTC+5:30, nishant wrote:

Why hydrotest pressure is taken 1.3 times of design pressure? What is the criteria that fixes the term 1.5 times or 1.25 times, etc.???

Thanks in advance,
Nishant nair
Sent from Yahoo! Mail

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...