Wednesday, May 28, 2014

[MW:20910] Use of ER 320 LR instead of ERNiCrMo-18 for Alloy 20 (UNS 08020)

Can some one share his/her experience for the welding of SB463 UNS 08020? i.e. for welding of butt welds what shall be consumables?
As per API 582 Table B2- ER 320LR for overlay on CS/LAS & as per ASME Sec IIC, SFA 5.11/5.14 ERNi Cr Mo-18.

Regds/Jignesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...