[MW:20882] RE: 20879] LTCS wps revised to CS

Dear you can revise WPS and can make many WPS, but tin this case electrode / filler material is essential variable, therefore, need to re qualify it again as per ASME IX.

 

A.Raza

KSA Jubail

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of S.Mohammed
Sent: Monday, May 26, 2014 8:21 AM
To: materials-welding@googlegroups.com
Subject: [MW:20879] LTCS wps revised to CS

 

Dear all

Have WPS P1G1 to P1G1
for LTCS 333 gr6  with ER80Ni2.
Thk 1.5 to 11

Can i change/revised to WPS P1G1 to P1G1
For A106 grB with ER 70S2.
without PQR qualification.
Since both P n F number not.changed.

Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...