Re: [MW:20501] WPS base metal qualification range

If PQR is P15E+P4, then as per QW 424
It is qualified for
P15 E or P5B to any metal with in P4.


On Sun, Apr 6, 2014 at 8:18 AM, Binoy Lonappan <binoypl3@gmail.com> wrote:
As per Section IX QW 424 for procedure qualification it is given thatt

for base material range of qualification as P15 E metal to P4 metal is
qualified for any metal from P15E to P4 or P3,P1
But P number is an essential variable so what is the actual
interpretation of the above clause

Or does it means if we qualify procedure for P15E +P4 then it is
qualified for the P15E any metal from this group to any metal from
P4,P3 P1 groups

--
With Regards
Binoy Lonappan
+91-9645100560
QAC Engineer
TECCL

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...