less than 5%------ Low alloy
5 to less than 10.50%-- Medium alloy
>-10.50 -----------High alloy
THANKS & BEST REGARDS
KG.PANDITHAN, AWS-CWI, CSWIP 3.1
CONSULTANT-WELDING & QUALITY
On Thu, Apr 3, 2014 at 6:01 PM, Raghuram Bathula <raghurambathula@gmail.com> wrote:
pl. check previous discussions!https://groups.google.com/forum/?hl=en&fromgroups&nomobile=true#!searchin/materials-welding/low$20alloy$20steel%7Csort:relevance%7Cspell:true/materials-welding/OeN6eNgRi2o/OGtdBWiBTAYJ
On 3 April 2014 15:37, Binoy Lonappan <binoypl3@gmail.com> wrote:Dear all,What is the percentage of alloying element in low alloy steels and High alloy steels,If its given in any standards(ASME) kindly give the section & clause detailsis it below 10% or 7.5 % for low alloy steels----
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment