Friday, April 4, 2014

Re: [MW:20483] Regarding WPS Heat Input.

Dear Dindo,
 
Travel speed is 3.36 mm/sec,its not in mm/Min,
 
 
Dear Hegde,
 
Process is SMAW.(Downhill welding)
 
 
Regards
Prashun

On Thu, Apr 3, 2014 at 5:22 PM, Dindo <dindodelacruz@gmail.com> wrote:
I am assuming that the travel speed is 3.36 inch/min which is
equivalent to 85.344 mm/min

Formula is VA X 60 / TS X 1000
                    85(27) X 60 / 85.344 X 1000 = 1.6 KJ

I am not sure where you got the 0.68 from.



On Thu, Apr 3, 2014 at 6:58 AM, Prashun Kumar <prashunk@gmail.com> wrote:
> Dear All,
>
> As In site,
>
>
>
> Welding Inspector taking daily welding  parameters per pass each day   for
> WPS-01, currently for root, the welder is not able to meet the requirements
> of Min heat Input mentioned in the WPS.
>
> For example :As per WPS
>
> For root:
>
> Amperage:84-102
>
> Voltage:25.5-31.2
>
> Travel Speed:3.35-4.10.
>
> Heat Input(Min):0.710
>
>
>
> Welder welding in current: 85, Voltage:27, Travel speed:3.36, Heat
> Input:0.68 which is not meeting the min Heat Input range.(whether this
> should be accepted or rejected).Please clarify.
>
>
>
>  Reply given by -Welding Engineer in blue:   I suggest to increase the
> current  to slighter higher value without changing the voltage & travel
> speed.
>
>
>
>     Mr.Mani, we need to try best combination of parameters by varying
> current, voltage & travel speed within the parameters provided in WPS
> which are most suitable for all the welders in production welds.
>
>
>
>      Once you fix the particular Amps, Volts, travel speed, you need to
> check these parameter in actual production whether welders are
>
>      following the same.  In above example, i feel just by increasing the
> current slightly will solve your problem.
>
>
>
> Minimum variable range for amperage and voltage mentioned in the WPS is not
> meeting to achieve Min heat Input mentioned. If it is not achieving the Min
> heat input ,then why ranges for voltage and amperage  mentioned to follow
> the procedure.
>
> This was asked to  QA/QC Inspectors, they were unable to clarify.
>
>
>
>     WPS parameters are +/- 10% of PQR average values.
>
>
>
>    For getting min heat input, we should not multiply min current X min
> voltage/ Min Travel speed.
>
>
>
>    If we use above formula in writing WPS ranges, WPS parameters will not be
> actual paramters used in PQR qualification.
>
>
>
>
> Can anybody can clarify this for me: I m not satified with this answer :Can
> anbody explain me how the parameters are taken from PQR to make WPS.
>
> Regards,
>
> Prashun
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...