Afees,
This issue is discussed previously here, search this forum; you will get nice explanations given by experts.
ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,
Nandesh Kumar Arasappa
P.S. : Please don't print this e-mail unless you really need to.
--------------------------------------------
On Wed, 2/4/14, afees kareem <afeeskareem@gmail.com> wrote:
Subject: [MW:20461] Query On QW- 403.5
To: materials-welding@googlegroups.com
Date: Wednesday, 2 April, 2014, 2:57 PM
Dear al,
could anyone please explain this clause from QW -
403.5. " when base metals of two
different P-Number Group Number combinations are qualified
using a single test coupon, that coupon qualifies the
welding of those two P-Number Group Numbers to themselves as
well as to each other using the variables qualified."
i am not able to interpret the
correct meaning of it.
regards,Afees
--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members
personel views and meant for educational purposes only,
Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
---
You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35354] Cast-iron welding
1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-