Dear Sir,
This clause refers; for single pass and multi pass with 13mm and more deposition heat input increases and so base metal thk range is 1.1 times the qualified thk and such condition happens with SAW, GMAW, FCAW, SMAW processes only.
On Tuesday, April 1, 2014 11:52:19 AM UTC+5:30, Sandeep Maan wrote:
-- This clause refers; for single pass and multi pass with 13mm and more deposition heat input increases and so base metal thk range is 1.1 times the qualified thk and such condition happens with SAW, GMAW, FCAW, SMAW processes only.
On Tuesday, April 1, 2014 11:52:19 AM UTC+5:30, Sandeep Maan wrote:
Dear expertCan anybody tell me the meaning of qw 403.9for single pass or multipass welding in which any pass is greater than 13mm thick, an increase in base metal thickness beyond 1.1 times that of the qualification test coupon.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment