Re: [MW:19741] Query-- Deformed Surface On 84" Damaged Elbow


Dear Shaikh Ahmed 

            Please specify the bend made by which process ( Hot induction or Hot forged ).

MADHUSOODHANAN NAIR


On Tue, Dec 24, 2013 at 12:37 PM, GENE MATSKO <g_matsko@yahoo.com> wrote:
It is the responsibility of the designer or operator to determine what minimum diameter he can tolerate.
Check B31.4 for information and tech. guidance. I hope this helps. 
Gene Matsko


On Monday, December 23, 2013 11:55 PM, shaikh ahmed <ahmedmech77@gmail.com> wrote:
Dear Expert,
 
Below Specified Elbows have deforms on surface. (Max. 5.5mm dent)
 
A234-WPB 84" 90D Elbow 12.7T 12Ea
 
cONSTRUCTION code B31.3 -pROCESS piping
 
84" 90 Degree LR Elbow having deformed surface. The pictures below  attached .
 
Request you to provide the Valuble Suggestion and action required to be taken and also provide any code code refernce.
 
thanks in advance for your valuable Suggestion.
 
 
 
  
 
 
 
 
 
Best Regards,
Suk-Hoo, HA (하석후)
Piping Supervisor / SADARA MFC Piping Dep't
A : P.O. Box 606, Jubail 31951 Daelim Saudi Arabia Co.,Ltd
M : (+)966 - (0)51 – 512 – 8037
Ext. : 151
DAELIM SAUDI ARABIA CO., LTD.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...