Re: [MW:19739] Duplex Grade UNS 31803 Weld - UT Velocity

YOU CAN CALCULATE ACTUAL VELOCITY IN THE MATERIAL.
BHASKAR

On Thu, Jan 2, 2014 at 9:38 AM, <think.differently360@gmail.com> wrote:
Saravanan,
The basic of UT sound of velocity of Steel alsmot same including SS and CS. But to know exactly you have to calib on standard block of which material to be used.

On Tuesday, December 17, 2013 6:56:13 PM UTC+7, saravanan sornam wrote:

Thank you Mr.Prem , do you have any material for my reference.
Regards
Saravanan
Korea

On Dec 17, 2013 1:38 AM, "prem nautiyal" <prem_na...@yahoo.com> wrote:
Hi
 
I think You can consider the velocity of sound as steel for this material.
For longitudinal waves, take V = 5900 m/sec
For shear waves, take V = 3200 m/sec
 
Regards
 
Prem Nautiyal
9769316004


On Monday, December 16, 2013 10:00 AM, Saravanan Sornam <sarava...@gmail.com> wrote:

Dear Experts ,

What is the Ultrasonic Velocity to be used for Duplex UNS 31803 material welding examination.

   Please share some data and material copy for my reference. 

Awaiting for your reply.

Thanks and Regards,
Saravanan,
Korea.


--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.


--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
धन्यवाद,
भास्कर मनोहर काळे
+60149129098

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...