Thursday, November 21, 2013

Re: [MW:19334] socket welding of steam pipe line

Most important issue for socket weld is gap between tube end with socket end should be 1.6 mm min
Eyup Tan



james gerald <gerry_tup@yahoo.com> yazdı:
If you weld small diameter and less thickness, TIG welding may be preferred.
 
Thanks & Regards


J.Gerald Jayakumar
00974-55835810


On Thursday, November 21, 2013 1:28 PM, Prabir Kumar Singh <prabirkumarsingh86@gmail.com> wrote:
Dear All

In socket welding of high pressure steam pipeline we have to weld by
SMAW . But our Client ask us, first pass of welding should be by  TIG
welding. Then SMAW welding. Is TIG welding necessary in socket
welding. Please suggest with any code reference

With Regards:
Prabir Kumar Singh

--
Sent from Kaiten Mail. Please excuse my brevity.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...