Saturday, August 31, 2013

[MW:18549] Need supplier address for induction heating

Dear experts,

I need one help from you,We are in need to pre- heat the valve body by induction heating method before production welding. Do you have any supplier in india & abroad ? to design & supply the induction pre heating system (System consists of power source,water cooled  flexible coil, thermo-couple with digital thermo meter and necessary items) for our application.
Our valve body material will be : ASTM A 216-WCB,A217-WC6,WC9 & C12A
Pre heating temperture will be 100,150,200DegC
Kindly do the needful to proceed further.

Regards,
sankaran.Sp
welding & metallurgy expert