Re: [MW:17527] Name Plate Hydro Test pressure

Dear Mr. Prem,

Test pressure given in drawing i.e. at vertical position shall be mentioned in Name Plate.

Regards,
Ajay Pathak


On Tue, Apr 23, 2013 at 2:08 PM, prem_nautiyal26 <prem_nautiyal26@yahoo.com> wrote:
Hello Mr Ghosh


I am very much aware that a vertical vessel can be hydrotested in horizontal position , but my question is what pressure should be mentioned on name plate : the corrected i.e tested pressure or the one mentioned in drawing for vertical position ??

Regards 

Prem Nautiyal


Sent from Samsung Mobile

Tarantula Ghosh <ghosh.tarantula@gmail.com> wrote:
Mr Prem,

Hope this helps:
Interpretation:        VIII-1-95-27
Subject:        Section VIII, Division 1 (1992 Edition, 1993 Addenda); UG-99(b)
Date Issued:    January 12, 1995
File:        BC94-414

Question (1):     Does the last sentence of UG-99(b) of Section VIII, Division 1, "All loadings that may exist during this test shall be given consideration," require that the static head that exists in a tower in the vertical position must be considered when determining the test pressure in the horizontal position?                     Reply (1):     No.

Question (2):     Does UG-99 specify in which position a vertical tower must be hydrotested?     Reply (2):     No.


T Ghosh


On Mon, Apr 22, 2013 at 9:41 PM, prem nautiyal <prem_nautiyal26@yahoo.com> wrote:
Hi friends
 
Vendor has fabricated a process equipment with skirt support as per ASME Sec VIII Div.1
 
The height is 11 metres and ID is 4.5 metres.
 
The vessel is going to be erected at site in vertical position with skirt supports.
The HydoTest Pressure specified on drawing for Vertical position is 14.5 Kg/cm2g.
 
However Due to shop height restriction vendor is not able to conduct Hydro Test in Vertical position and  has done hydro test in horizontal position  adding the head difference ( for every 10 m height - 1 Kg/cm2g head to be added).
So the actual Hydro Test Pressure conducted in shop is at 15.5 Kg/cm2g.
Also he has mentioned the corrected hydro test pressure i.e. 15.5 Kg/cm2g on Name Plate.
Nothing is mentioned about this corrected pressure in drawing or QAP.
 
Is it correct ?
 
Does the fabricator have to mention the actual tested corrected  hydrotest pressure on Name Plate or the Pressure mentioned on drawing.
Please give code reference.
 
Regards
 
Prem Nautiyal
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
Tarantula



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...