As Mr Pal written, temp is restricted as per 31.3
Pandithan
welding consultant
On 3/27/13, Biplab Pal <biplab.mech@googlemail.com> wrote:
> Dear Mohd.,
>
> As per ASME B-31.3 Table 331.1.1 you have to do PWHT within the specified
> range of 593 deg C to 649 deg C (for P-No-1) you can not do or write beyond
> that limits.
>
>
>
> On Sat, Mar 23, 2013 at 10:20 AM, mohd <mohd52100@gmail.com> wrote:
>
>>
>> Dear all,
>>
>> WPS details as per ASME IX Design Code :B31.3
>>
>> 1) GTAW + SMAW (3mm+ 24mm)
>> 2) Material API 5L x52 Thk : 26.97
>> 3) PWHT 600 +/-20 Time : 1Hr 20min
>> 4) No impact.
>>
>> Can I Re Write WPS with Temperature 670+/-20 as per As per QW-407.1 a
>> (2)
>> ? ( up to below Lower transformation no need re qualification )
>>
>> Need expert Opinion.
>>
>> ( QW-407 Postweld Heat Treatment
>> QW-407.1 A separate procedure qualification is
>> required for each of the following:
>> (a) For P-Numbers 1 through 6 and 9 through 15F materials,
>> the following postweld heat treatment conditions
>> apply:
>> (1) no PWHT
>> (2) PWHT below the lower transformation temperature )
>>
>>
>>
>> Regards,
>> mohd.
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>>
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>
>> The views expressed/exchnaged in this group are members personel views
>> and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>> ---
>> You received this message because you are subscribed to the Google Groups
>> "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an
>> email to materials-welding+unsubscribe@googlegroups.com.
>> For more options, visit https://groups.google.com/groups/opt_out.
>>
>>
>>
>
>
>
> --
> Thanks & Regards
> Biplab Pal
> Welding Inspector
> E-mail: biplab.mech@gmail.com
>
> Information in this email and any attachments is confidential and intended
> solely for the use of the individual(s) to whom it is addressed or
> otherwise directed. Please note that any views or opinions presented in
> this email are solely those of the author and do not necessarily represent
> those of the Company. Finally, the recipient should check this email and
> any attachments for the presence of viruses. Myself accepts no liability
> for any damage caused by any virus transmitted by this email.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment