Re: [MW:17217] IGC Practice A and E

Hi,
 
IGC Testing Practice A is Oxalic Acid Etch Test for Classification of Etch Structures of Austenitic Stainless Steels.
 
and
 
Practice E is Copper–Copper Sulfate–Sulfuric Acid Test for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels
 
So as indicated above, Practice A is rapid method of identifying, by simple etching, those specimens of certain stainless steel grades that are essentially free of susceptibility to intergranular attack associated with chromium carbide precipitates. As a result of this some specimens can be acceptabe and does not need further testing (B,C,E,F). Hence first this test is carried out for each material at first when Owner doesnot specify anything.
 
However in most cases owner specifies Practice E for Austenitic Stainless Steel.
 
Hope this helps.
 
 
Regards;
 
 
Purav Desai.
 
 
 
On Mon, Mar 25, 2013 at 8:19 PM,  <fsachin@gmail.com> wrote:
> You can perform both Pracice A as well E for SS. Basicallly it is as per the requirement of service condtion which tobe decided by designer/Clinet at per bid level. Please refer ASTM A262 for details.
>
> ----------
> Sent via Nokia Email
>
> ------Original message------
> From: Venkatesh <vpv_333@yahoo.com>
> Date: Sunday, March 24, 2013 11:18:59 PM GMT-0700
> Subject: [MW:17211] IGC Practice A and E
>
> Dear Expert,
>  
> What is the difference between IGC practice 'A' and 'E'?
>  
> Which is recommended for Austenitic stainless steels?
>
> Thanks & Regards
>
> P.Venkatesh
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
 
 
 
--
Regards;
 
Purav DESAI
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...