Friday, March 22, 2013

Re: [MW:17199] How to make WPS & PQR

Thank you sir
Your attachments are really help to me. Actually I was very confused that how to refer the codes because there is lots of articles and I was not sure to which I should take and which one not, but now I got the link to start my study.
Thank you very much sir

On Mar 22, 2013 3:21 PM, "Nandesh Kumar" <nandeshkumar@rocketmail.com> wrote:

Useful link :

http://www.wes.ir/files/2326318welding%20qualification.pdf

Also see attached

Also, you can search this forum. Many experts have given answers to your query clearly.


ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,

Nandesh Kumar A

Abu Dhabi, UAE

P.S. : Please don't print this e-mail unless you really need to.


--- On Fri, 22/3/13, BRIJESH KUMAR SINGH <brijeshkumarsingh1986@gmail.com> wrote:

From: BRIJESH KUMAR SINGH <brijeshkumarsingh1986@gmail.com>
Subject: Re: [MW:17192] How to make WPS & PQR
To: materials-welding@googlegroups.com
Date: Friday, 22 March, 2013, 6:35 AM

Sir
You can consider ASME.
Please tel me sir I want it for study purpose.
I am thankfull for  you response.

On Mar 22, 2013 11:04 AM, "Subramaniyan Karunanidhi" <subrakaruna@gmail.com> wrote:
Hi,
Based on what code?
Regards,
Karun

On Fri, Mar 22, 2013 at 1:38 AM, BRIJESH KUMAR SINGH <brijeshkumarsingh1986@gmail.com> wrote:

Dear seniors
I regularly fallow your all E-mails and query. Can any bady tel me how to prepare WPS & PQR.
I will really appropriate you if anyone help me for the above.

Thanks in advance

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...