Friday, March 22, 2013

Re: [MW:17198] How to make WPS & PQR

Dear Mr. brijeshkumarji,


Please visit the following site for to making and review WPS/PQR....

www.wpsamerica.com

Regards,
hemal chauhan,
Engineers india limited



From: Dinesh <som.din@gmail.com>
To: materials-welding@googlegroups.com
Sent: Friday, 22 March 2013 2:31 PM
Subject: RE: [MW:17195] How to make WPS & PQR

Dear sir,
 
Please read asme 9 & along with aws d1.1.First read aws d 1.1 so it will be easy to understand an some sort of information.
 
Regards
Dinesh
 
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of chandrakant mohikar
Sent: Friday, March 22, 2013 10:32 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:17193] How to make WPS & PQR
 
You need to specify co. requirements for preparation.
 
you may refer
 
QW 100, 200 articles in ASME sec. IX
 
Chandrakant Mohikar (PMC)
(ex. Project-QA, PDO/ VELOSI Oman)
 
On Thu, Mar 21, 2013 at 11:08 PM, BRIJESH KUMAR SINGH <brijeshkumarsingh1986@gmail.com> wrote:
Dear seniors
I regularly fallow your all E-mails and query. Can any bady tel me how to prepare WPS & PQR.
I will really appropriate you if anyone help me for the above.
Thanks in advance
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...