Re: [MW:17164] HAZ hardness

Dear all,

I completely agree your point that variation in grain structure affects the hardness. But the thing is that in welding HAZ is subjected to repeatative number of heat cycles which results in grain coarsening of HAZ. So, are coarse grain responsible for high hardness of HAZ?
Thanks and regards,


On Tue, Mar 19, 2013 at 6:27 PM, paragpan@gmail.com <paragpan@gmail.com> wrote:
Dear Hrushikesh,

It is due to the distortion of grain structure occurred during welding in the HAZ area due to heat transfer from the molten weld metal to the base metal.

Regards,

PARAG

Sent from my HTC


----- Reply message -----
From: "Hrushikesh Sangamnerkar" <hrushi612@gmail.com>
To: <materials-welding@googlegroups.com>
Subject: [MW:17145] HAZ hardness
Date: Mon, Mar 18, 2013 10:50 PM



Dear sir,

Why is the Hardness of HAZ higher than that of Weld?


Thanks and Regards,
Hrushikesh H Sangamnerkar
09724738118

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
Hrushikesh H Sangamnerkar
09724738118

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...