Tuesday, January 8, 2013

Re: [MW:16465] UT of anchor flange

U won't be able to peform ut on the area what u have mentioned below.

Regards

Nitin

On Jan 4, 2013 9:12 AM, "Samun Bhatia" <samunbhatia@gmail.com> wrote:
dear all,

we need to carry out UT on anchor flange of pipeline as per drawing.

in the weld neck portion due to the taper profile we are not getting any echo while using TR & straight proble.

so in this neck portion what is the method of UT ? do we have to use angle probe ?


please reply in detail.

regards,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate