Re: [MW:16453] Preheating regards Tensile strength

Dear Mr.Naresh
 

330.1.1 Requirements and Recommendations.

Required and recommended minimum preheat temperatures

for materials of various P-Numbers are given in

Table 330.1.1. If the ambient temperature is below 0°C

(32°F), the recommendations in Table 330.1.1 become

requirements.

 

Regards
Muthu



On Sun, Jan 6, 2013 at 12:56 PM, Naresh Kumar <snareshkumar30@yahoo.com> wrote:

 
Dear experts,
Asper ASME31.3 table 330.1.1 preheating should be done for all thickness(79 deg C), if tensile strength of base metal exceeds 490MPA.In my project we have 2"OD  and 5.54 thickness with 510MPA tensile strength(Base metal).
 In this case whether preheating is require or not. Kindly give some suggestions.
Thanks & Regards,
Naresh


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...