Hardness comes down appreciably after PWHT, and this is required. Teat treatment (PWHT) is mostly done as a mandatory procedure in P91steel. Check your client requirements for hardness after PWHT



From: Ryan Carbonara <rcarbonara@valv.com>
To: materials-welding@googlegroups.com
Sent: Thursday, January 3, 2013 8:51 AM
Subject: [MW:16412] RE: 16411] HardnessP-91 Material

Client call typically. You wont find it in B31.1
 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Anthony Rudder
Sent: Wednesday, January 02, 2013 11:37 AM
To: materials-welding@googlegroups.com
Subject: [MW:16411] HardnessP-91 Material
 
Sir,
What's the Max hardness for weld metal and HAZ for P-91 Material per B31.1
 
 
 
 
Thank You,
 
Tony
QA.Manager.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...