Saturday, January 5, 2013

Re: [MW:16444] Difference between the electrode E8018 B-8 & E8015 B-8

Attached may be useful to you.

ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,

Nandesh Kumar A

Abu Dhabi, UAE

P.S. : Please don't print this e-mail unless you really need to.


--- On Sat, 5/1/13, Biplab Pal <biplab.mech@googlemail.com> wrote:

From: Biplab Pal <biplab.mech@googlemail.com>
Subject: [MW:16440] Difference between the electrode E8018 B-8 & E8015 B-8
To: "materials-welding" <materials-welding@googlegroups.com>, "JALADHAR JENA" <jdjena2006@yahoo.co.in>, "Pinaki Boxi" <boxi.pinaki@gmail.com>, "chandan.majumdar" <chandan.majumdar@sgs.com>
Date: Saturday, 5 January, 2013, 5:50 AM

Dear Experts,

Can any body differentiate between the electrodes E8018 B-8 & E8015 B-8, and the difference of applicable areas.

--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...