Sunday, January 6, 2013

Re: [MW:16442] HardnessP-91 Material

Hi Tony

You may refer to your client specs..but mostly for P91 the hardness value in Hv10 is :
Weld metal 190 - 320
Base Metal 190 - 265

On Jan 3, 2013 11:20 AM, "Anthony Rudder" <ARudder@irwinindustries.com> wrote:

Sir,

What's the Max hardness for weld metal and HAZ for P-91 Material per B31.1

 

 

 

 

Thank You,

 

Tony

QA.Manager.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...