yes, you can use for with out impact test.
 
Pramodh

From: MUTHUKUMARAN M.P.N <m.p.n.muthu@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, January 3, 2013 2:05 PM
Subject: Re: [MW:16423] P1-P1 qualified WPS for welding API 5L PSL2
Dear Mr.Krishna WPS can be used for welding API 5L pipes within Essential variables of ASME SEC.IX .
However it is not advisable to use for API 5L grade X60 & above as the min UTS of filler wire used will be less than the UTS of the base material.
regards
Muthu
On Wed, Jan 2, 2013 at 4:02 PM, krishna <wiqw@rediffmail.com> wrote:
Dear Team,

We have WPS/PQR for SA106 Gr.B(P1-P1) whether this shall be used for welding of API 5L PSL2
seamless & welded pipes for production and welder qualification.

pls share your experiences.

thanks,
krishna

Catch India as it happens with the Rediff News App. To download it for FREE, click here
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 
-- To post to this group, send email to materials-welding@googlegroups.comTo unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.comFor more options, visit this group's bolg at http://materials-welding.blogspot.com/http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.  

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...