[MW:16515] PWHT/SR FOR IS 2062 Material.

Dear Sir
 
Is it necessary to do PWHT/SR  for IS2062 material . If so required , from whick thickness it should  be done & in which code it is mentioned .
 
please send me the details.
 
 
 
Thanking you
 
 
 
Yours Sincerely
 
Ch.v.v.n.kirankumar
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 