SIR
WE HAVE PRE QUALIFIED WPS WITH ASTM 106 OR EQUIVALENT MATERIAL P1 TO P1 . PROCESS GTAW, THICKNESS 1.5 TO 11.08.AS PER ASMESEC IX.
WE HAVE PIPES ASTM 53 Gr A GALVANIZED PIPE FOR HAND RAIL APPLICATION SCH.40 (3.67 MM) .IS THE ABOVE MENTIONED WPS IS COMPATIBLE FOR THIS APPLICATION OR NOT? THIS PIPES BECOMES THE PART OF STRUCTURAL ...SO CLIENT REQUIREMENT IS NEEDS WPS BASED ON AWS D1.1.
IS IT MANDATORY?
BASE METAL COMING UNDER P1 ..SO IS IT POSSIBLE TO APPLY HERE OR NOT.
PLS ADVICE.
--
-- WE HAVE PRE QUALIFIED WPS WITH ASTM 106 OR EQUIVALENT MATERIAL P1 TO P1 . PROCESS GTAW, THICKNESS 1.5 TO 11.08.AS PER ASMESEC IX.
WE HAVE PIPES ASTM 53 Gr A GALVANIZED PIPE FOR HAND RAIL APPLICATION SCH.40 (3.67 MM) .IS THE ABOVE MENTIONED WPS IS COMPATIBLE FOR THIS APPLICATION OR NOT? THIS PIPES BECOMES THE PART OF STRUCTURAL ...SO CLIENT REQUIREMENT IS NEEDS WPS BASED ON AWS D1.1.
IS IT MANDATORY?
BASE METAL COMING UNDER P1 ..SO IS IT POSSIBLE TO APPLY HERE OR NOT.
PLS ADVICE.
--
Thanks & Regards
PRADEEPKUMAR HORMIS
QC WELDING INSPECTOR
PRADEEPKUMAR HORMIS
QC WELDING INSPECTOR
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment