Monday, December 3, 2012

Re: [MW:16111] Advice on SS 316L sweep blast and Coal tar application

For Sweep blast,aluminium oxide or garnet is better choice because copper slag will penetrate more and contamination
Pandithan
welding consultant

On Sun, Dec 2, 2012 at 7:51 PM, Vajjiravelu Ravi <vajjiraveluravi3@gmail.com> wrote:
For SS -Instrument Air System IAS - buried pipe line - to be sweep blast and
 coal tar - cold wrapping to be applied
 To sweep blast SS 316L -aluminium oxide or garnet to be used as per  client specification -


 if copper slag used what will happen ( of course some
 contamination and earlier corrosion) but wish to know specific kindly advice if possible

--
Vajjiravelu Ravi

 
take all steps to save our health  wealth & environment.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...