Dear Mr. Goswami.
Thank you for your reply, but main worry is; can we apply UT for equipments in LETHAL SERVICE?
Code case 2235-9 is silent @ lethal service equipment?
Regards;
Purav Desai.
On Sun, Dec 2, 2012 at 12:09 AM, pgoswami <pgoswami@quickclic.net> wrote:
Hi Purav,PAUT or TOFD are accepted by ASME code in lieu of radiography for new construction..Please seethe attachment which references 3-ASME code cases.You may get these ASME documents in IHS website.Thanks.Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist
Ontario, Canada.
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Purav Desai
Sent: Friday, November 30, 2012 4:29 AM
To: materials-welding@googlegroups.com
Subject: [MW:16090] PAUT for Vessel in Lethal ServiceDear Member,Is it alllowed to use ultrasonic examination(PAUT) in lieu of Radiography for vessel intented to be used in lethal service?--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Regards;
Purav DESAI
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment