Wednesday, August 1, 2012

Re: [MW:14999] SS Electrode Eccentricity Tester

Dear Sir Sirdhar
Ok sir I am waiting for that device details.

Ahmad


From: c sridhar <sridhar305@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Tuesday, July 31, 2012 7:54 PM
Subject: Re: [MW:14997] SS Electrode Eccentricity Tester

Mr. Ahmd.

It is a dual checking meter used for both MS & SS.
It is an Indian product  and I will come back with details shortly.

sridhar.


From: Murtaza Ghauri <murtaza506@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Saturday, 28 July 2012 11:46 AM
Subject: Re: [MW:14972] SS Electrode Eccentricity Tester

Dear Sir,

Tell me the company name and product name(if any) whose electrode eccentricity tester you are using for SS electrode. 
the tester that we are using is only for electrodes containing MS core wire.

AHMAD

From: c sridhar <sridhar305@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Friday, July 27, 2012 7:35 PM
Subject: Re: [MW:14969] SS Electrode Eccentricity Tester

Mr. Ahmad,

The electrode  coating (eccentric)  testing is ment for all types of electrodes
including SS also.

We have used the tester for all types of electrodes in the plant.

sridhar.

From: Ahmad Ghauri <murtaza506@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Friday, 27 July 2012 4:01 PM
Subject: [MW:14968] SS Electrode Eccentricity Tester

Dear All

We have an eccentricity tester that determines the eccentricity of SMAW electrodes containing MS core wire.
Is there any tester that determines the eccentricity of SMAW electrodes containing SS core wire???


Regards,
AHMAD
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35763] Hardness range for CS+ Alloy0625 clad welding

Dear experts. I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. Both material consists of a base metal with alloy...