Re: [MW:15152] artificial defect

Dear Gerald
I want to qualify procedure according to ASME Sec V, but i don't now defects must be machined into the weld  or
natural.if natural how to be compared the real size with assesssed size?


From: james gerald <gerry_tup@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Tuesday, August 28, 2012 3:42 PM
Subject: Re: [MW:15144] artificial defect

It depends what type of defects you want to check.
 
Like porosity - you can use a wet electrode or long arc
Cracks            - Embed Copper wires on carbon steel plates and weld
Lack of Fusion  - Ask your welder to not to fuse the side wall of the Joint
 
Thanks & Regards

J.Gerald Jayakumar
00968-93281596
 
From: Ali Asghari <asghariali@rocketmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Tuesday, August 28, 2012 8:46 AM
Subject: [MW:15141] artificial defect

Dear All
We want to demonstrate a phased array procedure with welded samples that have defects.
Does anybody know procedure/informations about making a weld with defects for qualification of NDT procedure?
Regards.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...