Re: [MW:15096] joining of Carbon steel A36 to brass steel JIS BsC3

Dear Sridhar,
Thanks for your response.
Please refer the attachment.I have this details only.
Muthusamy.S
UAE

On 15 August 2012 07:11, c sridhar <sridhar305@yahoo.com> wrote:
Mr. Muthusamy,

A36 to brass JIS BsC3.

You have not mentioned the thickness factor, type of joint, application  etc

1. WPS or BPS : It is BPS  as braze welding / brazing depending upon the type of
                          joint, thickness
2. BPQ             : It is BPQ
3. filler classification....etc : The filler metal / flux combination after knowing
                                                the chemistry of JIS Bs C3, application  etc.

sridhar.
-----------------------------------------------------------------------------------------



From: Muthu Samy <jenieragav@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, 13 August 2012 11:41 AM
Subject: [MW:15075] joining of Carbon steel A36 to brass steel JIS BsC3



--
Dear Experts,
Please let me know the details for joining the carbon steel A36 to brass JIS BsC3.
1. WPS or BPS
2. BPQ
3. filler classification....etc
Thanks in advance

Muthusamy.S
UAE

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...