Dear Exparts,
I have a doubt on WQT!
Is it required to check all parameters stated in WPS during WQT? Ref:
Sec IX, 2010.
As we know " A WPS is a written qualified welding procedure prepared
to provide direction for making production welds to Code requirements.
The WPS or other documents may be used to provide direction to the
welder or welding operator to assure compliance with the Code
requirements.
Suppose we consider Welder Performance Qualification:
As per QW 350, the essential variables are very few and limited for
each process.
So, what parameters should an Inspector Check during Welder
Performance Qualification as per Sec IX, 2010.
Please give code reference for your statement.
--
Thanks & Regards
Biplab Pal
Mechanical Inspector (PMT)
YASREF Project
E-mail: biplab.mech@gmail.com
Information in this email and any attachments is confidential and intended
solely for the use of the individual(s) to whom it is addressed or
otherwise directed. Please note that any views or opinions presented in
this email are solely those of the author and do not necessarily represent
those of the Company. Finally, the recipient should check this email and
any attachments for the presence of viruses. Myself accepts no liability
for any damage caused by any virus transmitted by this email.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
I have a doubt on WQT!
Is it required to check all parameters stated in WPS during WQT? Ref:
Sec IX, 2010.
As we know " A WPS is a written qualified welding procedure prepared
to provide direction for making production welds to Code requirements.
The WPS or other documents may be used to provide direction to the
welder or welding operator to assure compliance with the Code
requirements.
Suppose we consider Welder Performance Qualification:
As per QW 350, the essential variables are very few and limited for
each process.
So, what parameters should an Inspector Check during Welder
Performance Qualification as per Sec IX, 2010.
Please give code reference for your statement.
--
Thanks & Regards
Biplab Pal
Mechanical Inspector (PMT)
YASREF Project
E-mail: biplab.mech@gmail.com
Information in this email and any attachments is confidential and intended
solely for the use of the individual(s) to whom it is addressed or
otherwise directed. Please note that any views or opinions presented in
this email are solely those of the author and do not necessarily represent
those of the Company. Finally, the recipient should check this email and
any attachments for the presence of viruses. Myself accepts no liability
for any damage caused by any virus transmitted by this email.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments