Dear Experts,
 
        Can any one explain me difference between %ferrite, Delta ferrite and FN(Ferrite Number).
My requirement in job was 5 to 10 delta ferrite. I procured consumable of 5.4 FN. And I am actually getting value 14 by ferritoscope.
Can anyone explain reason.?
--
With Best Regards

Mohammed Raza Rajani
Engineer - Q.C
Email ; rezarajani@gmail.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...