Re: [MW:15102] Ferrite Number

Dear,

There are many factors affecting ferrite measurement by ferritoscope.

1) Check the calibaration 
2) Adopt the correct method of measurement 
3) More often pple measure the ferrite on grinded/machined surface which shows high ferrite no exactly in a range what you land up in(12-14%).

There is a negligible  variation in ferrite no and percent so up to 10 you can consider both as a same.

Regards,
VJ

On Tue, Aug 21, 2012 at 4:04 PM, Mohammed Reza Rajani <rezarajani@gmail.com> wrote:

Dear Experts,
 
        Can any one explain me difference between %ferrite, Delta ferrite and FN(Ferrite Number).
My requirement in job was 5 to 10 delta ferrite. I procured consumable of 5.4 FN. And I am actually getting value 14 by ferritoscope.
Can anyone explain reason.?
--
With Best Regards

Mohammed Raza Rajani
Engineer - Q.C
Email ; rezarajani@gmail.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...