Thursday, August 23, 2012

Re: [MW:15115] electrode with diff impact temp mixing during welding.

Dear Member,
 
Hope the following from ASME Sec II will help.
 
 
A6.10.3 Toughness. Charpy V-notch impact requirements
are included in the specification. All classes of electrodes
in the specification can produce weld metal of
sufficient toughness for many applications. The inclusion
of impact requirements for certain electrode classifications
allows the specification to be used as a guide in selecting
electrodes where low-temperature toughness is required.
There can be considerable variation in the weld metal
toughness unless particular attention is given to the welding
procedure and the preparation and testing of the specimens.
The impact energy values are for Charpy V-notch specimens
and should not be confused with values obtained
with other toughness tests.
 

Regards
Sandeep Mehta
Mo : 09825736574

------------------------------------------------------------------------
  The information transmitted is intended only for the person or entity
  to which it is addressed and may contain confidential and/or privileged
  material. Any review, retransmission, dissemination or other use of, or
  taking of any action in reliance upon, this information by persons or
  entities other than the intended recipient is prohibited. If you received
  this in error, please contact the sender and permanently delete the
  material from any computer.
------------------------------------------------------------------------



On Wed, Aug 22, 2012 at 3:16 PM, mohd <mohd52100@gmail.com> wrote:
dear experts,

We have land in difficult situtuation due to welders mistakes.

Electrode E7018H4R impact require -46deg but by mistakes welder used
some electrodes E7018H4R -29deg during welding of 3 long seam 25m
(filling n caping)

Materials      516 gr 60    thk 40t.
Process        GTAW+SMAW

 What could be solution? To save joint.
Client already given cut out.

Regards,
Mohammed.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...