Sunday, August 26, 2012

[MW:15130] Hardness Test on Incoloy 825 / Equotip 3 Machine

Dear Experts,
 
We are not able to find any setting of Incoloy 825 in said machine for checking the hardness after PWHT on Vessel.
Hope you can help us out...or suggest other alternate method to check hardness..
 
Note: The Vessel is at Site and requires Portable machine.
 
Regards
Vino, Doha
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...