Pl. check impact properties of electrodes at -46deg in same grade of steel
as per SEC-II Part-C.
If it is ok than you can confirm to your client.
Otherwise, go for rework.
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of mohd
Sent: Wednesday, August 22, 2012 11:46 AM
To: Materials & Welding
Subject: [MW:15103] electrode with diff impact temp mixing during welding.
dear experts,
We have land in difficult situtuation due to welders mistakes.
Electrode E7018H4R impact require -46deg but by mistakes welder used
some electrodes E7018H4R -29deg during welding of 3 long seam 25m
(filling n caping)
Materials 516 gr 60 thk 40t.
Process GTAW+SMAW
What could be solution? To save joint.
Client already given cut out.
Regards,
Mohammed.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=
anet_ug_hm
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
as per SEC-II Part-C.
If it is ok than you can confirm to your client.
Otherwise, go for rework.
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of mohd
Sent: Wednesday, August 22, 2012 11:46 AM
To: Materials & Welding
Subject: [MW:15103] electrode with diff impact temp mixing during welding.
dear experts,
We have land in difficult situtuation due to welders mistakes.
Electrode E7018H4R impact require -46deg but by mistakes welder used
some electrodes E7018H4R -29deg during welding of 3 long seam 25m
(filling n caping)
Materials 516 gr 60 thk 40t.
Process GTAW+SMAW
What could be solution? To save joint.
Client already given cut out.
Regards,
Mohammed.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=
anet_ug_hm
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments