Dear Exparts,
In refinery construction i have seen somewere PWHT is the service
requirement for piping.
I had a idea that PWHT is the requirement of Welding to improve the
Impact properties of Joints.
Can anybody give me any idea, why PWHT is done in service of fluid
other than impact properties.
--
Thanks & Regards
Biplab Pal
Mechanical Inspector (PMT)
YASREF Project
E-mail: biplab.mech@gmail.com
Information in this email and any attachments is confidential and intended
solely for the use of the individual(s) to whom it is addressed or
otherwise directed. Please note that any views or opinions presented in
this email are solely those of the author and do not necessarily represent
those of the Company. Finally, the recipient should check this email and
any attachments for the presence of viruses. Myself accepts no liability
for any damage caused by any virus transmitted by this email.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
In refinery construction i have seen somewere PWHT is the service
requirement for piping.
I had a idea that PWHT is the requirement of Welding to improve the
Impact properties of Joints.
Can anybody give me any idea, why PWHT is done in service of fluid
other than impact properties.
--
Thanks & Regards
Biplab Pal
Mechanical Inspector (PMT)
YASREF Project
E-mail: biplab.mech@gmail.com
Information in this email and any attachments is confidential and intended
solely for the use of the individual(s) to whom it is addressed or
otherwise directed. Please note that any views or opinions presented in
this email are solely those of the author and do not necessarily represent
those of the Company. Finally, the recipient should check this email and
any attachments for the presence of viruses. Myself accepts no liability
for any damage caused by any virus transmitted by this email.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments