Dear Haja M Before analising the cause following data is important i) What is the base material and its chemistry ii) Was the plate tested by UT,MP on Weld edge before Welding iii)How the eqpt was loaded during PWHT , Does it have adequet movent facilty during PWHT due to expansion iv) What is the welding parameter used , and consumable chemistry, Does weld tested by UT before PWHT some time RT will not reveal CRack in the weld. iv) Does Eqpt have restraint joint near the seam v) Does the crack is longitudinal along the weld (In weld ) or in HAZ,Does it have transvers net work of crack All such information is very essential to analyse, Only the cooling rate of such a small deviation will not cause such a long crack Regards Hegde P.B. --- On Tue, 31/7/12, haja jaindeen <mhmj2k@yahoo.com> wrote:
|
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments