Dear,
STRAIGHTNESS
Pipe smaller than size 4
1/2 shall be reasonably straight. All other pipe shall be randomly checked for straightness; deviation from a straight line shall not exceed 0.2% of the length. Measurement may be made using a taut string or wire from end to end along the side of the pipe, measuring the greatest deviation. M Veera SAMY- Bureau Veritas. Coimbatore
Thank & Best Regards,
Date: Tue, 21 Aug 2012 13:15:16 +0300
Subject: [MW:15098] pipe angular distortion acceptance limits..
From: ranmi2007@gmail.com
To: materials-welding@googlegroups.com
Dear Experts,
Can any body tell pipe angular distortion acceptance limits..
Regards,
YEM
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments