test those electrodes for impact at -46 °C and convince your client.
On Aug 22, 11:16 am, mohd <mohd52...@gmail.com> wrote:
> dear experts,
>
> We have land in difficult situtuation due to welders mistakes.
>
> Electrode E7018H4R impact require -46deg but by mistakes welder used
> some electrodes E7018H4R -29deg during welding of 3 long seam 25m
> (filling n caping)
>
> Materials 516 gr 60 thk 40t.
> Process GTAW+SMAW
>
> What could be solution? To save joint.
> Client already given cut out.
>
> Regards,
> Mohammed.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:35668] Selection of Filler/Electrode.
Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment