Mr.Suresh,
please maintain preheat 100-150 deg c and interpass temperature 250 deg min.
Date: Thu, 23 Aug 2012 17:30:41 +0530
Subject: [MW:15117] cause of crack
From: sureshndb@gmail.com
To: materials-welding@googlegroups.com
Dear Members,
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
please maintain preheat 100-150 deg c and interpass temperature 250 deg min.
Thank & Best Regards,
M Veera SAMY- Bureau Veritas.
Coimbatore
Date: Thu, 23 Aug 2012 17:30:41 +0530
Subject: [MW:15117] cause of crack
From: sureshndb@gmail.com
To: materials-welding@googlegroups.com
Dear Members,
we found some weld cracks on parent metal (adjacent to weld bead) after weeding and depth of the crack is max 20 mm from the edge of the plate.
i would like to know the type of crack and causes of the crack.
please see the attached pictures.
Material:- IS 2062 Gr B to Itself
Thickness:- 25mm to 25mm
Joint Type:- Closed Corner
Grove Type:-Single side bevel
Electrodes:- E 7018
Preheating:- 80 to 100 Deg Cent
Electrodes Baking:- As per manufacturer recommendations.
waiting for your valuable reply.
Thanks and Regards,
Suresh,
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.