Weld a Test Coupon with same lot number of Electrodes (-29C Impact Tested). and get it Impact tested from lab at -46C. it will solve problem.
-- On Wed, Aug 22, 2012 at 2:09 PM, Chan, David <David.Chan@exterran.com> wrote:
Mohammed,I think it is a honest mistake and to avoid future problems, it is advisable to cut it out and re-weldo with full compliance the approved WPS. The responsibility is too huge to shoulder. I think it is an appropriate decision
Sent from Samsung Mobile
mohd <mohd52100@gmail.com> wrote:dear experts,
We have land in difficult situtuation due to welders mistakes.
Electrode E7018H4R impact require -46deg but by mistakes welder used
some electrodes E7018H4R -29deg during welding of 3 long seam 25m
(filling n caping)
Materials 516 gr 60 thk 40t.
Process GTAW+SMAW
What could be solution? To save joint.
Client already given cut out.
Regards,
Mohammed.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments