Dear suresh
First of all check if all parameters of WPS are followed..once this is confirmed n found ok check for WEP,as this seems a lameller tearing..so instead of making single side groove on one part,suggested to have WEP inclusive of both the part..i am sure your problem will not repeat..

On Aug 23, 2012 10:10 PM, "suresh" <sureshndb@gmail.com> wrote:
Dear Members,
we found some weld cracks on parent metal (adjacent to weld bead) after weeding and depth of the crack is max 20 mm from the edge of the plate.
i would like to know the type of crack and causes of the crack.
please see the attached pictures.

Material:- IS 2062 Gr B to Itself
Thickness:- 25mm to 25mm
Joint Type:- Closed Corner 
Grove Type:-Single side bevel
Electrodes:- E 7018
Preheating:- 80 to 100 Deg Cent
Electrodes Baking:- As per manufacturer recommendations.
waiting for your valuable reply.

Thanks and Regards,
Suresh,


 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...