Thursday, March 29, 2012

Re: [MW:14015] Speed of Tensile Test

Dear Puspraj,

I think following answer satisfies your query :

Tensile strength increases but ductility decreases as the testing speed is increased. The speed of the cross head of the tensile machine therefore needs to be controlled and BS EN 10002 specifies a stress rate range of 6MPa per second to 60MPa per second. The ASTM specifications have similar - but not identical - requirements.

jk70f4.gif
                                                                   Effect of speed of testing on strength and ductility

 

On Wed, Mar 28, 2012 at 5:09 PM, Pushpraj Anand <pushprajanand34@gmail.com> wrote:
What is the speed of tensile test for Procedure qualification as per section IX?

i read some coads they recommended for some speed of tensile test,is
it mandatory to follow or we can do at any speed?
--
Regards,
Pushpraj Anand

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...