Re: [MW:14012] Can SMAW welders qualified in matl Grade A36 weld also S355 ..ASME section IX

All materials comes under same P number. So no need to qualify again.
 
Arvinda

On Tue, Mar 27, 2012 at 10:19 AM, Anthony <hepolitodias@gmail.com> wrote:
we generally have welders qualified to A36 in our firm as per sec
presently we are working on a project demanding S355 JR /JO and we
have qualified the procedure and wleders also but can i use my other
welders who are qualified in A36[3G]  and A106 Gr B [6G] as per ASME
sec IX

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...