Hi mauricio,
 
Yes PWHT is required in this case.
 
Thanks
Ravish

On Tuesday, December 20, 2011 9:06:31 AM UTC+5:30, Raghuram Bathula wrote:
Yes it is required for Thickness > 0.75" (20mm)

On Tue, Dec 20, 2011 at 4:43 AM, mauricio padilla <mauricio_padilla_f@yahoo.com> wrote:
Dear,
 
Please I need your Help, about ASME B31,3.
 
I need to know if it is required PWHT.
 
CASE:
 
Pipe A106 Grb (PN 1)
wall thickness  0.844"
 
B31.3
 
Chapter V
 
Table 331.1.1
 
According to table 331.1.1 really is it necessay PWHT.
 
Please tell me
 
Is it correct?.
 
Best regards
 
Mauricio
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...