Friday, March 23, 2012

Re: [MW:13981] Filler for Monel to carbon steel

Hi!
Best filler is ER NiCu7 for monel to monel and discimilar metal welding
Regards
Hegde P.B.
08805593046

--- On Thu, 22/3/12, Dsunil <dsunil@gicongoa.com> wrote:

From: Dsunil <dsunil@gicongoa.com>
Subject: [MW:13970] Filler for Monel to carbon steel
To: materials-welding@googlegroups.com
Date: Thursday, 22 March, 2012, 10:57 PM

Dear Experts,

 

Can  you recommend the filler in ER series  for welding  Monel 400  to  Carbon Steel (A105)  material.

 

Thanks and regards

S G Dixit

Sr. Manager- Materials

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...